Package Type |
N/A Tote |
Concentrate Appearance |
N/A Amber Liquid |
Dilution Appearance |
N/A Translucent |
Specific Gravity at 60ºF (15.6ºC) |
N/A 0.965 to 0.985 |
pH at 20:1 Ratio |
N/A 9.3 pH |
BRIX Factor |
N/A 1.2 |
Applications |
N/A
Hysol SL 36 XBB is specifically designed for machining of cast iron and low-medium alloyed steel, but also suited for low to moderate duty machining of aluminum alloys. Suggested Applications Grinding: Cast iron, low-medium alloyed steel, high alloyed stainless steel Milling, Turning: Cast iron, low-medium alloyed steel Drilling: Cast iron, low-medium alloyed steel Reaming, Tapping: Cast iron Broaching: Cast iron Possible Applications* Grinding: Aluminum alloys Milling, Turning: High alloyed stainless steel, aluminum alloys Drilling: High alloyed stainless steel, aluminum alloys Reaming, Tapping: Low-medium alloyed steel, aluminum alloys Broaching: Low-medium alloyed steel |
General Machining |
N/A 5 to 10 % |
Grinding |
N/A 4 to 6 % |
Water Range |
N/A CaCO3: 50-400 ppm |
Features and Benefits |
N/A
|
Storage and Handling |
N/A To avoid product deterioration always keep the container/drum tightly sealed. Store the product in a cool, dry place away from direct sunlight. Prevent exposure to frost and avoid water ingress. For optimum product stability, it is preferable to store the product indoors between 5°C and 45 °C / 41°F and 113°F. |